Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.320 - 1.71 J/cm | 0.600 - 3.20 ft-lb/in | Average value: 0.912 J/cm Grade Count:33 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.107 - 1.71 J/cm | 0.200 - 3.20 ft-lb/in | Average value: 1.02 J/cm Grade Count:67 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |