Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | >= 0.107 J/cm | >= 0.200 ft-lb/in | ASTM D256 |
S&E Specialty Polymers GPP1005HF Series PP Application: UL94 V-2, Flame-retardant polypropylene compounds for injection molding applications.Information provided by S&E Specialty Polymers |
|||
Izod Impact, Notched | 0.107 J/cm @Thickness 3.17 mm |
0.200 ft-lb/in @Thickness 0.125 in |
D 256 |
RTP Company RTP 400 FR Polystyrene (PS), Flame Retardant |
|||
Izod Impact, Notched | 0.107 - 2.14 J/cm | 0.200 - 4.00 ft-lb/in | Average value: 0.596 J/cm Grade Count:13 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Izod Impact, Notched | 0.107 - 2.14 J/cm | 0.200 - 4.00 ft-lb/in | Average value: 0.498 J/cm Grade Count:65 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Notched | 0.107 J/cm | 0.200 ft-lb/in | ASTM D256 |
Teknor Apex Synres® PP 70 MH13 MB Polypropylene Notes: The Specialty Compounding Division offer a proprietary line of flame retardant polyolefins. Typical applications include building products, electrical/electronic and many other consumer and i.. |
|||
Izod Impact, Notched | 0.107 J/cm | 0.200 ft-lb/in | |
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul.. |
|||
Izod Impact, Notched | 0.107 J/cm | 0.200 ft-lb/in | |
Tra-Con Tra-Bond 2103 Medium Viscosity/Low Vapor Pressure Epoxy Adhesive TRA-BOND 2103 is a clear, near transparent, medium viscosity epoxy adhesive formulation developed for rigid laminating, sealing and bonding applications where the combination of good wetting plus im.. |
|||
Izod Impact, Notched | 0.107 J/cm | 0.200 ft-lb/in | |
Tra-Con Tra-Bond 2125 Rigid Syntactic Repair Adhesive TRA-BOND 2125 is a medium viscosity, low density syntactic foam epoxy formulation developed for industrial, electronic and aerospace honeycomb, fillet, edge-fill, contour repair, bonding and casting.. |
|||
Izod Impact, Notched | 0.107 J/cm @Thickness 3.17 mm |
0.200 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers GPPS BEADS Injection Molding Grade, General Purpose Polystyrene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.107 J/cm @Thickness 3.17 mm |
0.200 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPS80-1800B Injection Molding Grade, General Purpose Polystyrene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.107 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.200 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers SAN 250 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 0.107 J/cm | 0.200 ft-lb/in | |
Atom Adhesives AA-BOND 2103 Epoxy Adhesive AA-BOND 2103 is a clear, near transparent, medium viscosity epoxy adhesive formulation developed for rigid laminating, sealing and bonding applications where the combination of good wetting and impr.. |
|||
Izod Impact, Notched | 0.107 J/cm | 0.200 ft-lb/in | |
Tra-Con Tra-Bond 2130 Medium Viscosity Epoxy Adhesive TRA-BOND 2130 is a clear, near transparent, medium viscosity epoxy adhesive formulation developed for rigid laminating, sealing and bonding applications where the combination of good wetting plus im.. |
|||
Izod Impact, Notched | 0.107 J/cm - NB | 0.200 ft-lb/in - NB | Average value: 0.913 J/cm Grade Count:165 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.107 - 1.71 J/cm | 0.200 - 3.20 ft-lb/in | Average value: 1.02 J/cm Grade Count:67 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |