Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF15 IM HS L 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF18 IM 511 18% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PC TL15 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm |
3.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN®-V 450 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® N120GL (COND, 50% RH) Nylon 6, 20% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 6510E Injection Molding Polypropylene Impact CopolymerApplications: General purpose injection molding of consumer products, household appliances, lawn and garden items and medical components.Formolene 6510E is a higher impact, medium st.. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | LAB034 |
ExxonMobil Mytex™ AS65KW-LGDC Talc filled compounded polypropylene produced for automotive interior applicationsInformation provided by ExxonMobil Chemical |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437M20L Mica Reinforced |
|||
Izod Impact, Notched | 1.98 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.70 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 7777 Rigid PVC, Extrusion Georgia Gulf 7777 is a rigid PVC compound designed for outdoor applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 1.98 J/cm | 3.70 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SBB 3707 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Medium Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provi.. |