Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Copolymer CP0437C40L Calcium Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
MD; ASTM D955
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Ash 40 %
40 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 44
44
ASTM D785
Tensile Strength at Break 11.0 MPa
1600 psi
ASTM D638
Tensile Strength, Yield 13.0 MPa
1890 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Tensile Modulus 1.500 GPa
217.5 ksi
ASTM D638
Flexural Strength 19.0 MPa
2760 psi
ASTM D790
Flexural Modulus 1.300 GPa
188.5 ksi
ASTM D790
Izod Impact, Notched 1.98 J/cm
3.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.2 °C
126 °F