Mechanical Properties Metric English Comments
Izod Impact, Notched 3.89 J/cm

@Temperature 23.0 °C
7.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS
LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t..
Izod Impact, Notched 3.89 J/cm

@Temperature 23.0 °C
7.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS (Asia Pacific)
LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t..
Izod Impact, Notched 3.89 J/cm
7.29 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL EN185 PPE+PS
Extrusion grade. Excellent impact strength. 185F (85C) DTUL. UL94 V-1 rated.