Polymer Property : Izod Impact, Notched = 5.60 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.44 - 5.60 J/cm
2.70 - 10.5 ft-lb/in
Average value: 3.77 J/cm Grade Count:3
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..