Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.59 J/cm | 6.73 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific) LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry. |