Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.95 J/cm @Temperature -10.0 °C |
13.0 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Izod Impact, Notched | 6.95 J/cm @Temperature -20.0 °C |
13.0 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 6.95 J/cm @Temperature -20.0 °C |
13.0 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 6.95 J/cm @Temperature -20.0 °C |
13.0 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 6.95 J/cm | 13.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® R3144 PC/PBT A thermoplastic alloy offering a high level of chemical resistance combined with high impact and excellent mechanical properties. Black.Data provided by the manufacturer |