Mechanical Properties Metric English Comments
Izod Impact, Notched 0.500 - 7.20 J/cm

@Temperature -30.0 - 0.000 °C
0.937 - 13.5 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 2.37 J/cm Grade Count:26
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..