Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2203-25 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-25 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Europe-Africa-Middle East) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PK2870 PC LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® PK2870 PC (Asia Pacific) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature -30.0 °C |
14.1 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature -30.0 °C |
14.1 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354 PC (Asia Pacific) This is a PC compound with good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 2061-15 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-15 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-15 provides excellent heat resistance, impact strength.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 302EP-22 Polycarbonate Resin Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ MEGARAD 2081-22 Polycarbonate Resin Overview: CALIBREâ„¢ 2081-22 polycarbonate resin is a high-flow resin designed for injection molded medical parts. It is stabilized to reduce color shift associated with exposure to high energy r.. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.20 mm |
14.1 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.20 mm |
14.1 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2405 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release, Makrolon grade 2458 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.20 mm |
14.1 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2458 Polycarbonate, Injection Grade Very easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Ba.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Engineered Plastics EPPC 1214C Polycarbonate Clear injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Engineered Plastics EPPC 1514G Polycarbonate Gray injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.17 mm |
14.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Makroblend® EL 703 Polycarbonate + Polyester-based Blend, Impact Modified, Flame-Retardant, UV Stabilized Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Engineered Plastics EPPC 2014B Polycarbonate Black injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Engineered Plastics EPPC 2014G Polycarbonate Gray injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 1061R Polycarbonate A general purpose polycarbonate, low melt flow for injection molding.Data provided by the manufacturer |