Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2204-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Asia Pacific) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX2614G PC (Europe-Africa-Middle East) Lexan LUX2614G (EXRL0944) is a diffusive, high viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develop.. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.17 mm |
14.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Bayblend® 2773 Polycarbonate + ABS Blend, Automotive
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Rostone Rosite® 3950ES SMC Thermoset Polyester, 25% Glass Reinforced
(discontinued **) Key Features: High Strength; High DielectricElectrical grade material that provides higher flexural and impact strength than Rosite 3550 composites with comparable glass fiber content. 3950ES is fo.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | >= 7.55 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 14.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 7.55 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature -30.0 °C |
14.1 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature -30.0 °C |
14.1 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Europe-Africa-Middle East) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature -30.0 °C |
14.1 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 203-22 Polycarbonate Resin Overview: CALIBREâ„¢ 200-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 2061-15 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-15 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-15 provides excellent heat resistance, impact strength.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 2091-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARADâ„¢ 2091 Polycarbonate Resins are designed for single use medical devices (SUDs) that require gamma and electron-beam irradiation and an accelerated schedule for de.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 200-23 Polycarbonate Resin Overview: CALIBREâ„¢ 200-23 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Izod Impact, Notched | 7.50 J/cm @Temperature 23.0 °C |
14.1 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ MEGARAD 2081-22 Polycarbonate Resin Overview: CALIBREâ„¢ 2081-22 polycarbonate resin is a high-flow resin designed for injection molded medical parts. It is stabilized to reduce color shift associated with exposure to high energy r.. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.20 mm |
14.1 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2405 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release, Makrolon grade 2458 for food contact applications.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was se.. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.20 mm |
14.1 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2407 Polycarbonate, Injection Grade Very easy flowing injection molding grade with easy mold release and UV stabilizer.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officia.. |
|||
Izod Impact, Notched | 7.50 J/cm @Thickness 3.20 mm |
14.1 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 2458 Polycarbonate, Injection Grade Very easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Ba.. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Engineered Plastics EPPC 1514B Polycarbonate Black injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Engineered Plastics EPPC 2014G Polycarbonate Gray injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Engineered Plastics EPPC 2214C Polycarbonate Clear injection grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | ASTM D256 |
Engineered Plastics EPPC 314C Polycarbonate Clear; extrusion/blow molding grade. Property values below represent typical values. Information provided by Engineered Plastics Corporation. |
|||
Izod Impact, Notched | 7.50 J/cm | 14.1 ft-lb/in | Notched/Unnotched not specified; ASTM D256 |
NOVA Chemicals Novapol® HB-W558-A HDPE Extrusion Resin
(discontinued **) Molded Plaque Properties. Features: High molecular weight, excellent impact strength, high rigidity, easy processing.Applications: large part blow molding, large oil drums.Data provided by the manu.. |
|||
Izod Impact, Notched | 7.52 J/cm | 14.1 ft-lb/in | |
Reliance Industries Polypropylene - 40% Glass filled Information provided by Reliance Industries |
|||
Izod Impact, Notched | 7.52 J/cm | 14.1 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXG154 PC (Asia Pacific) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended. |