Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.16 - 5.23 J/cm | 7.80 - 9.80 ft-lb/in | |
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression.. |