Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.54 J/cm | 8.50 ft-lb/in | Crosswise; ASTM D256 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
Izod Impact, Notched | 4.54 J/cm @Temperature 22.8 °C |
8.50 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Spartech PP7120 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Izod Impact, Notched | 4.54 J/cm | 8.50 ft-lb/in | 73°F; ASTM D256 |
Spartech Royalite R84 Weather Resistant Sheet Description: Weather Resistant SheetInformation provided by Spartech. |
|||
Izod Impact, Notched | 4.54 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
8.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 7600B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.54 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
8.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 9500B Description: Blow Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.54 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
8.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 9501 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.54 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
8.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 9502 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.54 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
8.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ABS 9502E Description: Extrusion Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.54 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
8.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA S190 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 4.54 J/cm | 8.50 ft-lb/in | Crosswise; ASTM D256 |
G-5 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and .. |
|||
Izod Impact, Notched | 4.54 J/cm | 8.50 ft-lb/in | Method A; ASTM D256 |
Phillips 66 COPYLENE® CM090L Polypropylene, High Impact Copolymer CM090L is a high impact copolymer with antistat and is specially designed to excel in injection molding processes for consumer products.Applications: Injection MoldingInformation provided by Phillip.. |