Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

G-9 Fiberglass Melamine Laminate Sheet

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Melamine
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF G-9 Fiberglass Melamine Laminate Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board panels, arc barriers, circuit breaker parts, and structural electrical parts. G-9 and similar fiberglass reinforced thermosets are sometimes known as garolite.Information provide by Boedeker Plastics.
Physical Properties Metric English Comments
Density 1.85 g/cc
0.0668 lb/in³
ASTM D792
Water Absorption 0.60 %
0.60 %
24 hrs.; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 115
115
ASTM D785
Tensile Strength at Break 352 MPa
51100 psi
Crosswise; ASTM D638
425 MPa
61600 psi
Lengthwise; ASTM D638
Flexural Strength 352 MPa
51100 psi
Crosswise; ASTM D790
425 MPa
61600 psi
Lengthwise; ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
Crosswise; ASTM D790
13.8 GPa
2000 ksi
Lengthwise; ASTM D790
Compressive Strength 448 MPa
65000 psi
ASTM D695
Izod Impact, Notched 4.54 J/cm
8.50 ft-lb/in
Crosswise; ASTM D256
6.67 J/cm
12.5 ft-lb/in
Lengthwise; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 14.9 µm/m-°C

@Temperature 20.0 °C
8.30 µin/in-°F

@Temperature 68.0 °F
Lengthwise; ASTM D696
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
Crosswise; ASTM D696
Thermal Conductivity 0.288 W/m-K
2.00 BTU-in/hr-ft²-°F
ASTM C177
Maximum Service Temperature, Air 140 °C
284 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 6.3

@Frequency 1e+6 Hz
6.3

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.8 kV/mm
300 kV/in
Short Time; 1/8 inch; ASTM D149
Dissipation Factor 0.019

@Frequency 1e+6 Hz
0.019

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Users viewing this material also viewed the following: