Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.81 J/cm | 9.01 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 5014 CU W Calcium Carbonate Filled Polypropylene Multi-Pro 5014 CU W is a calcium carbonate reinforced PP concentrate with balanced impact and stiffness properties. This product is specially formulated for lawn furniture, suitable for outdoor exp.. |
|||
Izod Impact, Notched | 4.81 J/cm | 9.01 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 40% long glass fiber reinforcementInformation provided by Plas.. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm |
9.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers ASAPC 122954H Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm @Thickness 3.17 mm |
9.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers ASAPC TA-45 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 4.81 J/cm | 9.01 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P114WO PBT Polyester A high impact polyester with low shrinkage, flame retardant.Data provided by the manufacturer |