Polymer Property : Izod Impact, Notched = 9.40 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 5.02 J/cm
9.40 ft-lb/in
ASTM D256
Ravago Manufacturing Americas Hysun™ A3525 ASA+PC
Available in North America Features: Good Impact Resistance RoHS CompliantForm: PelletsInformation provided by Ravago