Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.60 - 9.60 J/cm | 18.0 - 18.0 ft-lb/in | Average value: 9.60 J/cm Grade Count:4 |
Overview of materials for Polyphthalamide (PPA), High Impact This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, High Impact". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Notched | 0.320 - 9.60 J/cm | 0.599 - 18.0 ft-lb/in | Average value: 5.49 J/cm Grade Count:33 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |