Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.160 J/cm | 9.664 ft-lb/in | |
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro.. |