Mechanical Properties Metric English Comments
Izod Impact, Notched 5.28 J/cm

@Temperature 23.0 °C
9.89 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp DX93681 PC
LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 5.28 J/cm

@Temperature 23.0 °C
9.89 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Thermocomp DX93681 PC (Asia Pacific)
LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 5.28 J/cm
9.89 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA
Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications..