Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp DX93681 PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp DX93681 PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 56.0 MPa
8120 psi
ASTM D 638
Elongation at Break 63 %
63 %
ASTM D 638
Tensile Modulus 2.13 GPa
309 ksi
50 mm/min; ASTM D 638
Flexural Strength 82.0 MPa
11900 psi
ASTM D 790
Flexural Modulus 2.29 GPa
332 ksi
ASTM D 790
Izod Impact, Notched 5.28 J/cm

@Temperature 23.0 °C
9.89 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 122 °C

@Thickness 3.20 mm
252 °F

@Thickness 0.126 in
unannealed; ASTM D 648