Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.290 J/cm²

@Temperature -20.0 °C
1.38 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 GF 20 GB 10 PA6, 20% glass fibre, 10% glass beads
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre and 10% glass beads. Application: impacted mouldings and mouldings with high strength applied in automotive, electri..
Charpy Impact, Notched 0.290 J/cm²

@Temperature -30.0 °C
1.38 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® A CP400 (cond.) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact, Notched 0.290 J/cm²

@Temperature -30.0 °C
1.38 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® CST (cond.) Nylon 6/66
Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group.
Charpy Impact, Notched 0.290 J/cm²

@Temperature -30.0 °C
1.38 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® CST 38FL (cond.) Nylon 6/66
Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group.
Charpy Impact, Notched 0.290 J/cm²

@Temperature -30.0 °C
1.38 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DSM Akulon® S223-GM35 (Cond.) 15% Glass Reinforced, 25% Mineral Reinforced Nylon 66 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..