Charpy Impact, Notched 0.500 - 0.600 J/cm²

@Temperature 23.0 °C
2.38 - 2.86 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
Charpy Impact, Notched 0.350 - 0.600 J/cm²

@Temperature 23.0 °C
1.67 - 2.86 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group 5553 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..