Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.25 J/cm² @Temperature 23.0 °C |
5.95 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Stanyl® TW271F6J10 (PA46+PTFE)-GF30 30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Charpy Impact, Notched | 1.25 J/cm² @Temperature 23.0 °C |
5.95 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
BASF Ultramid® B3WG6 CR BK 23210 15% Glass Filled (Dry) Description: Ultramid B3WG6 CR BK23210 s a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade for crash relevant applications.Information provided by BASF |