Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.10 J/cm² @Temperature 23.0 °C |
14.8 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A HSX (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 3.10 J/cm² @Temperature 23.0 °C |
14.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PP TOUCH 25325 Polypropylene, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.10 J/cm² @Temperature 23.0 °C |
14.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PP TOUCH 25325 R3 Polypropylene, Glass Fiber Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.10 J/cm² @Temperature 23.0 °C |
14.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Solvay TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, Conditioned Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced po.. |
|||
Charpy Impact, Notched | 3.10 J/cm² @Temperature 23.0 °C |
14.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |