Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.60 J/cm² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S USZ200 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 3.60 J/cm² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical RS-650 ABS, Extrusion, General Purpose Information Provided by LG Chem |
|||
Charpy Impact, Notched | 3.60 J/cm² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1A |
Gromax BTE30-FN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 3.60 J/cm² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, Conditioned Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go.. |
|||
Charpy Impact, Notched | 3.60 J/cm² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Novamid® 1011CH5KR PA6 Heat Stabilized, Easy Molding Grade |
|||
Charpy Impact, Notched | 3.60 J/cm² @Temperature 0.000 °C |
17.1 ft-lb/in² @Temperature 32.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |