Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6/66 GF 50 PA6/66, 50% glass fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-g.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® S702 ABS (Europe-Africa-Middle East) CYCOLAC S702 is a high impact ABS combined with a good flow. This material is developed for enclosures and housings found in appliances and automotive industries.This data was supplied by SABIC-IP f.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPC GF7020 PD2 E15 Polypropylene Copolymer, Glass Fiber Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 HI-M PA6 with improved impact strength PA 6 with the content of thermoplastic elastomer. Impacted, for moldings with higher toughness even at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets, protecti.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Zytel® E51HSB NC010 is a high molecular weight, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-G8U (Dry) 43% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) Zytel® 73G30HSL NC010 is a 30% glass fiber reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided .. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature -20.0 °C |
9.99 ft-lb/in² @Temperature -4.00 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST7301 BK356 Nylon 6
(Unverified Data**) Zytel® ST7301 BK356 is a Super Tough, heat stabilized, lubricated, black polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and h.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1A |
Gromax ATE70-FN00N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East) XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 136Q32 Nylon 6, Injection Molding Grade SAXAMID 136Q32 is a high impact-modified polyamide 6 injection-molding-grade.Information provided by SAX Polymers |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-HG7 (Cond.) 35% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® S223-HG7 Nylon 66-35% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 22.8 °C |
10.0 ft-lb/in² @Temperature 73.0 °F |
Partial Break; ISO 179 |
ExxonMobil Exxtral™ BMV 301 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, designed for automotive interior application in which good surface finish, high s.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 22.8 °C |
10.0 ft-lb/in² @Temperature 73.0 °F |
Complete Break; ISO 179 |
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature -40.0 °C |
9.99 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® ST801AW NC010 Nylon 66
(Unverified Data**) Zytel® ST801AW NC010 is a Super Tough, high performance polyamide 66 resin. It is UV stabilized and when appropriately colored offers the best resistance to indirect sunlight in automotive interior.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecodur® PB70 GR20 NL IH PBT 20% glass fiber reinforced, impact modified Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, Conditioned Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, Conditioned Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-HG8 (Dry) 40% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® A ESL128 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature -30.0 °C |
9.99 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties... |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 23.0 °C |
9.99 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Stanyl® TS200F6 PA46-GF30 30% Glass Reinforced |
|||
Charpy Impact, Notched | 2.10 J/cm² @Temperature 20.0 °C |
9.99 ft-lb/in² @Temperature 68.0 °F |
ISO 179/1eA |
Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber Information provided by PolyPlastic Group. |