Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact, Notched = 2.38 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.350 - 0.500 J/cm²

@Temperature 23.0 °C
1.67 - 2.38 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group 2567 AMC
Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and ..
Charpy Impact, Notched 0.400 - 0.500 J/cm²

@Temperature 23.0 °C
1.90 - 2.38 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group 2568 AMC
Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s..
Charpy Impact, Notched 0.350 - 0.500 J/cm²

@Temperature 23.0 °C
1.67 - 2.38 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group RALUPOL® 4385 UP
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy..
Charpy Impact, Notched 0.350 - 0.500 J/cm²

@Temperature 23.0 °C
1.67 - 2.38 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group RALUPOL® 4806 UP
Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80..
Charpy Impact, Notched 0.350 - 0.500 J/cm²

@Temperature 23.0 °C
1.67 - 2.38 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group SURAPLAST 54 UPA
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
Copyright © lookpolymers.com All Rights Reserved