Polymer Property : Charpy Impact, Notched = 3.40 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.714 J/cm²

@Temperature 0.000 °C
3.40 ft-lb/in²

@Temperature 32.0 °F
ISO 179
ExxonMobil Exxtral™ BMU 141 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance and designed for automotive instrument panels in which good surface finish, high s..