Polymer Property : Charpy Impact, Notched = 3.80 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Cycolac® G320 ABS (Europe-Africa-Middle East)
CYCOLAC G320 is a super high impact resistant ABS grade. It combines impact resistance with high stiffness, good temperature resistance and processability. It has a good fit in automotive interiors ..
Charpy Impact, Notched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East)
XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
Charpy Impact, Notched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 4-8000 Polypropylene Random Copolymer
INNOPOL® CS 4-8000 is a polypropylene random copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 4-8000 is highly suitable for pressure pipe manufacturing, includi..
Charpy Impact, Notched 3.80 J/cm²

@Temperature 23.0 °C
18.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Styrolution Novodur® 4140PG ABS
Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by ..