Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | >= 15.0 J/cm² | >= 71.4 ft-lb/in² | ISO 179 |
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL C333/m² ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-20 Special low gloss grade for injection moulding which combines medium heat resistance with a good b.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² - NB | 71.4 ft-lb/in² - NB | Average value: 15.2 J/cm² Grade Count:21 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | |
Ineos ABS Lustran® M305 Grade for smart cards, good dimensional accuracy, excellent dynamic loading capacity.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | conditioned |
Ineos ABS Triax® KU2-3154 ABS + Nylon 6 Mineral reinforced, easy flowing, reduced moisture absorption, very low warpage, injection molding, pellets.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | ISO 179 |
Polyram Polytron A60N01 Nylon 6.6, 60% Long Fiber Glass 60% Long fiber glass reinforced natural Nylon 6.6, heat stabilized, for injection molding.Information provided by Polyram. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | ISO 179/1eU |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin 100TL is a high viscosity acetal homopolymer containing 1.5% Teflo.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | ISO 179 |
BASF Ultraform W 2320 003 UNC Q600 POM Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains .. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL is a high viscosity acetal homopolymer, containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.Inform.. |