Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | dry; ISO 179-1/1eU |
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² - NB | 71.4 ft-lb/in² - NB | Average value: 15.2 J/cm² Grade Count:21 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | |
Ineos ABS Lustran® M305 Grade for smart cards, good dimensional accuracy, excellent dynamic loading capacity.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature 23.0 °C |
71.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® KU 2-7205 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | ISO 179/1eU |
Covestro Desmopan® DP 3970D Polyurethane, 20% Glass Filled injection molding grade20 % Glass fiber reinforcedgood heat resistancelow coefficent of linear thermal expansionApplicationAutomotive engineeringInjection molded engineering partsPreprocessingMax. W.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSM-40/4 PA666-MD40 Product description: Grilon TSM-40/4 is a special heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 40% mineral filler. Grilon TSM-40/4 has the following important properties.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LKN-3H PA12-GB30 Product description: Grilamid LKN-3H is a 30% glass bead reinforced, heat stabilized polyamide 12 injection molding grade with the following property profile: Very low moisture absorptionExtremely g.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® 1C PA6/66 (Dry) Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | ISO 179 1eU |
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | ISO 179 |
BASF Ultraform W 2320 003 UNC Q600 POM Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains .. |
|||
Charpy Impact Unnotched | 15.0 J/cm² @Temperature -30.0 °C |
71.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform W 2320 003 UNC Q600 POM Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains .. |
|||
Charpy Impact Unnotched | 15.0 J/cm² | 71.4 ft-lb/in² | |
Polimeri Europa SINKRAL PD F332 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MGN,105-15-16-20 General purpose injection grade which combines excellent thermal stability during processing with.. |