Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.300 - 0.400 J/cm² | 1.43 - 1.90 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RALUPOL® 4566 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Charpy Impact Unnotched | 0.300 J/cm² - NB | 1.43 ft-lb/in² - NB | Average value: 7.79 J/cm² Grade Count:116 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact Unnotched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar.. |
|||
Charpy Impact Unnotched | 0.300 J/cm² | 1.43 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner PP8 PP For Automotive Parts Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact Unnotched | >= 0.300 J/cm² | >= 1.43 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.2 |
Hippe MF CC 201 Woven Cotton Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm). Arc and tracking resistant.Information provided by Hippe. |
|||
Charpy Impact Unnotched | 0.300 J/cm² - NB @Temperature -40.0 - -20.0 °C |
1.43 ft-lb/in² - NB @Temperature -40.0 - -4.00 °F |
Average value: 6.53 J/cm² Grade Count:61 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Charpy Impact Unnotched | 0.300 J/cm² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS NOVODUR® P2T ABS, Injection Grade
(discontinued **) Injection molding grade, very high heat resistance.Applications: Automotive industry, household appliances.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This g.. |