Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.550 J/cm² - NB
2.62 ft-lb/in² - NB
Average value: 14.1 J/cm² Grade Count:69
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Charpy Impact Unnotched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 2535 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof  (discontinued **
Phenolic molding compound, inorganically/organically filled, average heat resistant, steam resistant, dish washer proof, high surface quality.Application areas: Fittings for ovens and dishwashers, t..
Charpy Impact Unnotched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed  (discontinued **)
Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications..
Charpy Impact Unnotched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 14600 Phenolic Formaldehyde Resin, High Surface Quality  (discontinued **)
Phenolic molding compound, mainly organically filled, low specific gravity.Application areas: Cookware fittings, electric devices.Information provided by Bak AGBak AG became a part of Hexion in 2005..
Charpy Impact Unnotched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DSM Arnite® B604T PBT-I
Charpy Impact Unnotched 0.550 J/cm²

@Temperature 23.0 °C
2.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1/2 eU
Hexion Bakelite™ PF 2560 Phenolic Formaldehyde Resin, High Surface Quality, For Electrostatic Coating, UL Listed &n
Phenolic molding compound, inorganically/organically filled, average heat resistant, high surface quality, lower water absorption than PF 31, minimal distortion, UL listed molding compound 1.5 mm/V-..