Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.900 - 1.92 g/cc
0.0325 - 0.0694 lb/in³
Average value: 1.31 g/cc Grade Count:184
Water Absorption 0.000 - 0.600 %
0.000 - 0.600 %
Average value: 0.296 % Grade Count:77
Moisture Absorption at Equilibrium 0.0100 - 1.09 %
0.0100 - 1.09 %
Average value: 0.185 % Grade Count:69
Water Absorption at Saturation 0.100 - 0.500 %
0.100 - 0.500 %
Average value: 0.418 % Grade Count:17
Viscosity 1.60 - 400000 cP
1.60 - 400000 cP
Average value: 80000 cP Grade Count:5
8000 - 800000 cP

@Temperature 230 - 270 °C
8000 - 800000 cP

@Temperature 446 - 518 °F
Average value: 187000 cP Grade Count:2
8000 - 800000 cP

@Shear Rate 1.00 - 100000 1/s
8000 - 800000 cP

@Shear Rate 1.00 - 100000 1/s
Average value: 187000 cP Grade Count:2
Viscosity Test 105 - 180 cm³/g
105 - 180 cm³/g
Average value: 133 cm³/g Grade Count:15
Linear Mold Shrinkage 0.00160 - 0.0600 cm/cm
0.00160 - 0.0600 in/in
Average value: 0.0150 cm/cm Grade Count:136
Linear Mold Shrinkage, Transverse 0.00160 - 0.0240 cm/cm
0.00160 - 0.0240 in/in
Average value: 0.0145 cm/cm Grade Count:60
Melt Flow 3.00 - 236 g/10 min
3.00 - 236 g/10 min
Average value: 35.8 g/10 min Grade Count:92
Mechanical Properties Metric English Comments
Hardness, Rockwell M 72.0 - 90.0
72.0 - 90.0
Average value: 83.4 Grade Count:22
Hardness, Rockwell R 112 - 120
112 - 120
Average value: 117 Grade Count:21
Hardness, Shore D 40.0 - 87.0
40.0 - 87.0
Average value: 73.8 Grade Count:22
Ball Indentation Hardness 50.0 - 160 MPa
7250 - 23200 psi
Average value: 138 MPa Grade Count:13
Tensile Strength, Ultimate 8.00 - 165 MPa
1160 - 23900 psi
Average value: 50.5 MPa Grade Count:86
5.00 - 90.0 MPa

@Temperature -40.0 - 160 °C
725 - 13100 psi

@Temperature -40.0 - 320 °F
Average value: 38.8 MPa Grade Count:1
5.00 - 90.0 MPa

@Strain 2.00 - 10.0 %
725 - 13100 psi

@Strain 2.00 - 10.0 %
Average value: 38.8 MPa Grade Count:1
Tensile Strength, Yield 27.0 - 118 MPa
3920 - 17100 psi
Average value: 52.8 MPa Grade Count:111
22.0 - 105 MPa

@Temperature -40.0 - 100 °C
3190 - 15200 psi

@Temperature -40.0 - 212 °F
Average value: 63.5 MPa Grade Count:1
Elongation at Break 1.00 - 300 %
1.00 - 300 %
Average value: 69.4 % Grade Count:162
>= 100 %

@Temperature 60.0 - 120 °C
>= 100 %

@Temperature 140 - 248 °F
Average value: 100 % Grade Count:2
Elongation at Yield 2.90 - 75.0 %
2.90 - 75.0 %
Average value: 9.51 % Grade Count:76
Modulus of Elasticity 0.500 - 21.9 GPa
72.5 - 3180 ksi
Average value: 2.63 GPa Grade Count:95
0.180 - 0.900 GPa

@Temperature 60.0 - 120 °C
26.1 - 131 ksi

@Temperature 140 - 248 °F
Average value: 0.505 GPa Grade Count:2
Flexural Yield Strength 48.0 - 255 MPa
6960 - 37000 psi
Average value: 84.2 MPa Grade Count:104
25.0 - 25.0 MPa

@Temperature 90.0 - 90.0 °C
3630 - 3630 psi

@Temperature 194 - 194 °F
Average value: 25.0 MPa Grade Count:1
Flexural Modulus 1.42 - 17.9 GPa
206 - 2600 ksi
Average value: 2.49 GPa Grade Count:112
0.500 - 0.500 GPa

@Temperature 90.0 - 90.0 °C
72.5 - 72.5 ksi

@Temperature 194 - 194 °F
Average value: 0.500 GPa Grade Count:1
Izod Impact, Notched 0.265 - 8.02 J/cm
0.496 - 15.0 ft-lb/in
Average value: 1.38 J/cm Grade Count:85
1.86 - 6.94 J/cm

@Temperature -40.0 - -20.0 °C
3.48 - 13.0 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 3.51 J/cm Grade Count:2
1.30 - 5.70 J/cm

@Temperature -40.0 - -20.0 °C
2.44 - 10.7 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 3.51 J/cm Grade Count:5
1.30 - 5.70 J/cm

@Thickness 1.57 - 3.18 mm
2.44 - 10.7 ft-lb/in

@Thickness 0.0618 - 0.125 in
Average value: 3.51 J/cm Grade Count:5
Izod Impact, Unnotched 10.7 - 5340 J/cm
20.0 - 10000 ft-lb/in
Average value: 16.4 J/cm Grade Count:11
Izod Impact, Notched (ISO) 2.90 - 170 kJ/m²
1.38 - 80.9 ft-lb/in²
Average value: 24.1 kJ/m² Grade Count:23
3.00 - 22.0 kJ/m²

@Temperature -40.0 - -30.0 °C
1.43 - 10.5 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 7.20 kJ/m² Grade Count:6
Izod Impact, Unnotched (ISO) 80.0 kJ/m² - NB
38.1 ft-lb/in² - NB
Average value: 109 kJ/m² Grade Count:6
NB - NB

@Temperature -30.0 - -30.0 °C
NB - NB

@Temperature -22.0 - -22.0 °F
Grade Count:2
Charpy Impact Unnotched 0.550 J/cm² - NB
2.62 ft-lb/in² - NB
Average value: 14.1 J/cm² Grade Count:69
2.50 J/cm² - NB

@Temperature -30.0 - -20.0 °C
11.9 ft-lb/in² - NB

@Temperature -22.0 - -4.00 °F
Average value: 17.3 J/cm² Grade Count:51
Charpy Impact, Notched 0.120 - 1000 J/cm²
0.571 - 4760 ft-lb/in²
Average value: 1.40 J/cm² Grade Count:83
0.250 - 2.50 J/cm²

@Temperature -30.0 - -20.0 °C
1.19 - 11.9 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.841 J/cm² Grade Count:49
Gardner Impact 16.9 - 43.0 J
12.5 - 31.7 ft-lb
Average value: 29.5 J Grade Count:5
Tensile Impact Strength 65.0 - 160 kJ/m²
30.9 - 76.1 ft-lb/in²
Average value: 112 kJ/m² Grade Count:3
Dart Drop, Total Energy 100 - 140 J
73.8 - 103 ft-lb
Average value: 130 J Grade Count:4
Puncture Energy 6.90 - 45.0 J
5.09 - 33.2 ft-lb
Average value: 29.8 J Grade Count:8
2.00 - 32.0 J

@Temperature -30.0 - -30.0 °C
1.48 - 23.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 15.5 J Grade Count:6
Tensile Creep Modulus, 1 hour 1400 - 2800 MPa
203000 - 406000 psi
Average value: 2130 MPa Grade Count:16
Tensile Creep Modulus, 1000 hours 700 - 1800 MPa
102000 - 261000 psi
Average value: 1260 MPa Grade Count:20
Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1.20e+17 ohm-cm
100 - 1.20e+17 ohm-cm
Average value: 8.69e+15 ohm-cm Grade Count:110
Surface Resistance 100 - 2.00e+17 ohm
100 - 2.00e+17 ohm
Average value: 8.00e+15 ohm Grade Count:88
Dielectric Constant 2.90 - 4.00
2.90 - 4.00
Average value: 3.30 Grade Count:92