Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.780 - 8.79 J/cm² | 3.71 - 41.8 ft-lb/in² | Average value: 3.08 J/cm² Grade Count:28 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact Unnotched | 0.780 J/cm² @Temperature 23.0 °C |
3.71 ft-lb/in² @Temperature 73.4 °F |
EN ISO 179 |
Ensinger TECASINT™ 2032 Polyimide, Black, 40% Graphite (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Charpy Impact Unnotched | >= 0.780 J/cm² | >= 3.71 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.2 |
Hippe PF CC 202 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications (coarse weave: >130 g/m2, =30 threads/cm).Information provided by Hippe. |
|||
Charpy Impact Unnotched | 0.780 - 3.51 J/cm² | 3.71 - 16.7 ft-lb/in² | Average value: 1.87 J/cm² Grade Count:11 |
Overview of materials for Polyimide, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app.. |