Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.50 - 3.50 J/cm²

@Temperature -40.0 - -20.0 °C
16.7 - 16.7 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 3.50 J/cm² Grade Count:1
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 2.50 - 3.50 J/cm²
11.9 - 16.7 ft-lb/in²
Average value: 3.08 J/cm² Grade Count:6
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Charpy Impact Unnotched 3.50 - 3.50 J/cm²

@Temperature -30.0 - -30.0 °C
16.7 - 16.7 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.50 J/cm² Grade Count:1
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Charpy Impact Unnotched 3.50 - 3.50 J/cm²

@Temperature -30.0 - -30.0 °C
16.7 - 16.7 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.50 J/cm² Grade Count:1
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Charpy Impact Unnotched 0.780 - 3.51 J/cm²
3.71 - 16.7 ft-lb/in²
Average value: 1.87 J/cm² Grade Count:11
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..
Charpy Impact Unnotched 1.90 - 3.50 J/cm²
9.04 - 16.7 ft-lb/in²
Average value: 2.54 J/cm² Grade Count:9
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..
Charpy Impact Unnotched 2.60 - 3.50 J/cm²
12.4 - 16.7 ft-lb/in²
Average value: 3.03 J/cm² Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Charpy Impact Unnotched 2.20 - 3.50 J/cm²

@Temperature -40.0 - -30.0 °C
10.5 - 16.7 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 2.85 J/cm² Grade Count:2
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Charpy Impact Unnotched 3.00 - 3.50 J/cm²
14.3 - 16.7 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR F 4306 Bulk Molding Compound
Mechanical high grade standard productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion pr..
Copyright © lookpolymers.com All Rights Reserved