Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.65 J/cm² @Temperature -30.0 °C |
7.85 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1102 K Polypropylene Grade with high processing stability for film tape (low water carryover), fibrillated film, monofilaments, OPP film (special formulations) and thermoformed parts.Data was collected by ISO methods an.. |
|||
Charpy Impact Unnotched | 1.65 J/cm² @Temperature -30.0 °C |
7.85 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 1104 K Polypropylene Data was collected by ISO methods and provided by BASF. |