Charpy Impact Unnotched 1.65 J/cm²

@Temperature -30.0 °C
7.85 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1102 K Polypropylene
Grade with high processing stability for film tape (low water carryover), fibrillated film, monofilaments, OPP film (special formulations) and thermoformed parts.Data was collected by ISO methods an..
Charpy Impact Unnotched 1.65 J/cm²

@Temperature -30.0 °C
7.85 ft-lb/in²

@Temperature -22.0 °F
BASF Novolen® 1104 K Polypropylene
Data was collected by ISO methods and provided by BASF.