Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | |
Polimeri Europa EDISTIR RC3 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-18 Special high impact, high gloss polystyrene grade. Suitable for injection molding in the appliances sector.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 50/TF/15/NAT Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | ISO 179-1 |
Unitika A1030TF PA6, Conditioned Lubricating nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
|
BASF Polystyrol® 2710 Impact Grade Polystyrene (Europe) Special high-impact grade for refrigerators and the packaging sector. Particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 12.0 J/cm² @Temperature -30.0 °C |
57.1 ft-lb/in² @Temperature -22.0 °F |
|
BASF Polystyrol® 2712 Impact Grade Polystyrene (Europe) Easy flowing special grade, particularly resistant to stress cracking.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | |
BASF Polystyrol® 454 C Impact Grade Polystyrene (Europe) Easy flowing, medium-impact grade.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | DAM; ISO 179/1eU |
DuPont Performance Polymers Minlon® 12T BKB100 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T BKB100 is a 36% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Pe.. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | |
Polimeri Europa EDISTIR SRL550 High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,E,083-12-07-18 High impact, easy flow polystyrene with good elasticity at low temperatures. Used for sheet extrusion and .. |
|||
Charpy Impact Unnotched | 12.0 J/cm² | 57.1 ft-lb/in² | ISO 179/1eU |
Borealis Xmod™ MC55T1 Polypropylene Compound 10% Mineral Filled Xmod MC55t1 is a 10% mineral filled grade based on HCPP intended for injection molding. Xmod has been developed especially for the car industry, to be used in interior parts. XMod offers very good .. |