Material Notes:
Product description: Grilon TSM-40/4 is a special heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 40% mineral filler. Grilon TSM-40/4 has the following important properties: Excellent flow behaviorGood surface finishLow warpageEasy processing Application examples are injection molding parts which demand a good surface finish such as engine covers, fuel tank flaps, and wheel caps.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Water Absorption 6.0 %
6.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
conditioned; ISO 527-1/-2
90.0 MPa
13100 psi
dry; ISO 527-1/-2
Elongation at Break 7.0 %
7.0 %
dry; ISO 527-1/-2
22 %
22 %
conditioned; ISO 527-1/-2
Tensile Modulus 3.80 GPa
551 ksi
conditioned; ISO 527-1/-2
6.00 GPa
870 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
dry; ISO 179/1eU
15.0 J/cm²
71.4 ft-lb/in²
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
dry; ISO 179/1eA
0.500 J/cm²
2.38 ft-lb/in²
conditioned; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
38.9 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
38.9 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
180 °C
356 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Descriptive Properties Value Comments
Form Granules
Processing Injection Molding