Polymer Property : Charpy Impact Unnotched = 19.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.00 - 19.0 J/cm²

@Temperature -30.0 - 30.0 °C
9.52 - 90.4 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 4.92 J/cm² Grade Count:32
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..