Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne LubriOne™ NN-25GB/15T Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -40.0 °C |
13.3 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HH-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | ISO 179 |
Nilit Nilamid B G6 FR C4 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -40.0 °C |
13.3 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 FK 2010 Nylon 6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -40.0 °C |
13.3 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit RECONYL A GV30 Recycled nylon 6.6 for injection molding, 30% glass fiber reinforced Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1850-7784 PBT, with glass fiber, glass spheres and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 80-7580/BK Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East) VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | |
BASF Polystyrol® 168 N Polystyrene (Europe) High molecular, heat-resistant grades used where high strength is required. Suitable for expanded film.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature 23.0 °C |
13.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GS 25 HWCP 25% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 2.80 J/cm² @Temperature -30.0 °C |
13.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Charpy Impact Unnotched | 2.80 - 5.00 J/cm² | 13.3 - 23.8 ft-lb/in² | Average value: 4.14 J/cm² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Charpy Impact Unnotched | 2.80 J/cm² | 13.3 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Charpy Impact Unnotched | 2.80 - 5.30 J/cm² | 13.3 - 25.2 ft-lb/in² | Average value: 4.40 J/cm² Grade Count:24 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |