Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | >= 21.0 J/cm² | >= 99.9 ft-lb/in² | ISO 11542/2 |
Polikim ULPOLEN® 1000 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Charpy Impact Unnotched | 21.0 - 26.0 J/cm² @Temperature -30.0 - -30.0 °C |
99.9 - 124 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 22.8 J/cm² Grade Count:4 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Charpy Impact Unnotched | 21.0 J/cm² | 99.9 ft-lb/in² | |
Ineos ABS Lustran® E401 Very high surface resistance, high surface gloss.,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 21.0 J/cm² | 99.9 ft-lb/in² | ISO 179 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |