Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 21.2 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 4.45 - 7.60 J/cm²

@Temperature -30.0 - 30.0 °C
21.2 - 36.2 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 5.68 J/cm² Grade Count:6
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched 4.45 J/cm²

@Temperature -30.0 °C
21.2 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AUM 30 T6LD Nylon 12, 30% Glass Bead Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-020,GB30Rigid grad with glass beads filler (30%) for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Reinforce..
Copyright © lookpolymers.com All Rights Reserved