Overview of materials for Nylon 12, Glass Bead Filled

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Glass Bead Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 12, Glass Bead Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.21 - 1.44 g/cc
0.0437 - 0.0520 lb/in³
Average value: 1.32 g/cc Grade Count:6
Water Absorption 0.800 - 1.20 %
0.800 - 1.20 %
Average value: 1.05 % Grade Count:4
Melt Flow 5.00 - 70.8 g/10 min
5.00 - 70.8 g/10 min
Average value: 37.9 g/10 min Grade Count:4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 39.0 - 52.0 MPa
5660 - 7540 psi
Average value: 46.5 MPa Grade Count:6
Elongation at Break 18.0 - 32.0 %
18.0 - 32.0 %
Average value: 22.8 % Grade Count:6
Elongation at Yield 4.00 - 10.0 %
4.00 - 10.0 %
Average value: 6.25 % Grade Count:6
Modulus of Elasticity 1.60 - 3.64 GPa
232 - 528 ksi
Average value: 2.37 GPa Grade Count:6
Charpy Impact Unnotched 3.80 - 17.0 J/cm²
18.1 - 80.9 ft-lb/in²
Average value: 10.1 J/cm² Grade Count:6
4.45 - 7.60 J/cm²

@Temperature -30.0 - 30.0 °C
21.2 - 36.2 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 5.68 J/cm² Grade Count:6
Charpy Impact, Notched 0.420 - 0.560 J/cm²
2.00 - 2.67 ft-lb/in²
Average value: 0.490 J/cm² Grade Count:6
0.300 - 0.460 J/cm²

@Temperature -30.0 - 30.0 °C
1.43 - 2.19 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.380 J/cm² Grade Count:6
Thermal Properties Metric English Comments
CTE, linear 60.0 - 140 µm/m-°C
33.3 - 77.8 µin/in-°F
Average value: 97.5 µm/m-°C Grade Count:4
Melting Point 174 - 178 °C
345 - 352 °F
Average value: 175 °C Grade Count:6
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 68.0 °C
122 - 154 °F
Average value: 60.8 °C Grade Count:4
Flammability, UL94 HB
HB
Grade Count:6
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Average value: 1.00e+13 ohm-cm Grade Count:4
Surface Resistance 1.00e+12 - 1.00e+13 ohm
1.00e+12 - 1.00e+13 ohm
Average value: 5.50e+12 ohm Grade Count:4
Dielectric Strength 35.0 - 40.0 kV/mm
889 - 1020 kV/in
Average value: 37.5 kV/mm Grade Count:4
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:4