Mechanical Properties Metric English Comments
Charpy Impact Unnotched >= 30.0 J/cm²

@Temperature -40.0 - -20.0 °C
>= 143 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 30.0 J/cm² Grade Count:2
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched >= 30.0 J/cm²
>= 143 ft-lb/in²
DIN 53453
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)  (discontinued **)
Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper..
Charpy Impact Unnotched 30.0 J/cm²

@Temperature 23.0 °C
143 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro..
Charpy Impact Unnotched 30.0 J/cm²

@Temperature 23.0 °C
143 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal Homopolymer  (Unverified Data**)
Delrin® 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers, pigmented red, having extremely low VOC emissions, developed for automotive interior applicatio..
Charpy Impact Unnotched >= 30.0 J/cm²

@Temperature 23.0 °C
>= 143 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LATAN 23 Polyoxymethylene Copolymer (POM)  (discontinued **)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Charpy Impact Unnotched 30.0 J/cm²
143 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 100P BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved ProcessingDelrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100P provides maximum toughness in the product line..
Charpy Impact Unnotched 30.0 J/cm²

@Temperature -30.0 °C
143 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
DuPont Performance Polymers Delrin® 100PE BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100PE BK602 (formerly DE20573) is a high viscosity acetal homopolymer an enhanced version of Delrin 100P with very low VOC emissions...
Charpy Impact Unnotched 30.0 J/cm²
143 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 300PE NC010 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE NC010 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low..
Charpy Impact Unnotched 30.0 J/cm²
143 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It..
Charpy Impact Unnotched 30.0 J/cm²
143 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 527UVE RD402 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 527UVE RD402 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers pigmented red with very ..
Charpy Impact Unnotched 30.0 J/cm²
143 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati..
Charpy Impact Unnotched 30.0 J/cm²
143 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider..
Charpy Impact Unnotched 30.0 J/cm²
143 ft-lb/in²
ISO 179/1eU
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Charpy Impact Unnotched 30.0 J/cm²
143 ft-lb/in²
DAM; ISO 179/1eU
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info..
Charpy Impact Unnotched 30.0 J/cm²

@Temperature -30.0 °C
143 ft-lb/in²

@Temperature -22.0 °F
ISO 179
BASF Ultraform N 2640 Z4 UNC Q600 POM
Ultraform N2640 Z4 UNC Q600 is a high toughness, elastomer-modified injection molding POM grade.
Charpy Impact Unnotched >= 30.0 J/cm²

@Temperature -40.0 - -20.0 °C
>= 143 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 30.0 J/cm² Grade Count:1
Overview of materials for Low Density Polyethylene (LDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum ..
Charpy Impact Unnotched 30.0 J/cm² - NB

@Temperature -40.0 - -20.0 °C
143 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 30.0 J/cm² Grade Count:2
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..