Mechanical Properties Metric English Comments
Charpy Impact Unnotched 6.87 J/cm²

@Temperature -30.0 °C
32.7 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AZM 15 TLD Nylon 12, 15% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLR,16-030,GF15Rigid grade with glass fiber filler (15%) for injection molding.Available color: natural. Light and heat stabilized. Mold-release agent.Rigidity combined wi..
Charpy Impact Unnotched 6.87 J/cm²
32.7 ft-lb/in²
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
Charpy Impact Unnotched 6.87 J/cm²

@Temperature -30.0 °C
32.7 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Dry)
Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..