Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.50 - 8.70 J/cm²

@Temperature -30.0 - -30.0 °C
16.7 - 41.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.29 J/cm² Grade Count:9
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Charpy Impact Unnotched 0.400 - 8.70 J/cm²

@Temperature -40.0 - -20.0 °C
1.90 - 41.4 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.42 J/cm² Grade Count:56
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..