Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 1.90 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.400 - 0.600 J/cm²

@Temperature 23.0 °C
1.90 - 2.86 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eU
Raschig Group 4552 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Injection; ISO 179/1eU
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²

@Temperature 23.0 °C
1.90 - 2.86 ft-lb/in²

@Temperature 73.4 °F
Injection and Compression; ISO 179/ 1eU
Raschig Group EPOXIDUR® 3580 EP Epoxy
Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod..
Charpy Impact Unnotched 0.400 - 0.700 J/cm²
1.90 - 3.33 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group MELOPAS® 156 MF Melamine
Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200..
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
Compression; ISO 179/1eU
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..
Charpy Impact Unnotched 0.400 - 5.00 J/cm²

@Temperature -40.0 - -20.0 °C
1.90 - 23.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 2.36 J/cm² Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe..
Charpy Impact Unnotched 0.400 - 2.50 J/cm²
1.90 - 11.9 ft-lb/in²
Average value: 1.38 J/cm² Grade Count:4
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Charpy Impact Unnotched 0.400 - 1.50 J/cm²
1.90 - 7.14 ft-lb/in²
Average value: 0.928 J/cm² Grade Count:10
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
Charpy Impact Unnotched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1eU
Gromax BPR20-N1 Nylon 6, Flame Retardant (Dry)
Information provided by Gromax Enterprises Corp.
Charpy Impact Unnotched 0.400 J/cm²
1.90 ft-lb/in²
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer
High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific..
Charpy Impact Unnotched 0.400 J/cm²
1.90 ft-lb/in²
LATI Laticonther 52/11 GR/70 PP Homopolymer
High thermal conductivity product based on Polypropylene homopolymer (PPh). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat..
Charpy Impact Unnotched 0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
Styrolution NOVODUR® P2HGV ABS, 16% Glass Fiber
Injection molding grade, glass reinforced (16%).Applications: Automotive industry: instrument panels, rear light housings, internal components of domestic appliances.
Charpy Impact Unnotched 0.400 - 0.600 J/cm²
1.90 - 2.86 ft-lb/in²
ISO 179
Vyncolit X658 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by ..
Charpy Impact Unnotched 0.400 J/cm²
1.90 ft-lb/in²
IS0179-1:2000
Zhejiang Juner PP201-G30 PP For Automotive Parts
Applications: FansInformation provided by Zhejiang Juner New Materials Co, Ltd.
Charpy Impact Unnotched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
Notched/Unnotched not specified; ASTM DIN53453
Total PPC 4720 WZ Polypropylene, Impact Copolymer
ATOFINA 4720 is an impact copolymer. 4720 is characterized by a high fluidity offering a combination of east of processing and good mechanical properties.ApplicationATOFINA 4720 has been formulated..
Charpy Impact Unnotched 0.400 J/cm² - NB
1.90 ft-lb/in² - NB
Average value: 7.75 J/cm² Grade Count:49
Overview of materials for Nylon 6, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v..
Charpy Impact Unnotched 0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
LATI LARTON CE/60 60% Special Mineral Filled Polyphenylene sulfide (PPS)  (Unverified Data**)
Description: Larton thermoplastics are polyphenylene sulfide (PPS) products. They are distinguished by a group of very interesting properties combined with easy moldability. Larton parts feature: ex..
Charpy Impact Unnotched 0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
Ineos ABS NOVODUR® P3T ABS, Injection Grade  (discontinued **)
Injection molding grade, higher heat resistance.Applications: Automotive industry.Information provided by the manufacturer.Novodur is produced by Styrolution (2014). This grade was discontinued pri..
Charpy Impact Unnotched 0.400 - 6.00 J/cm²
1.90 - 28.6 ft-lb/in²
Average value: 2.56 J/cm² Grade Count:22
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 0.400 - 0.700 J/cm²

@Temperature -40.0 - -40.0 °C
1.90 - 3.33 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 0.550 J/cm² Grade Count:1
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact Unnotched 0.400 - 1000 J/cm²
1.90 - 4760 ft-lb/in²
Average value: 0.975 J/cm² Grade Count:5
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..
Charpy Impact Unnotched 0.400 - 8.70 J/cm²

@Temperature -40.0 - -20.0 °C
1.90 - 41.4 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.42 J/cm² Grade Count:56
Overview of materials for Polypropylene with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i..