Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.90 J/cm² | 42.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 216 V33 PA66, 33% glass fiber, DRY Description: TECHNYL® A 216 V33 is a polyamide 66, reinforced with 33% of glass fiber, for injection molding. This product is available in natural color.Benefits: The product offers an excellent .. |
|||
Charpy Impact Unnotched | 8.90 J/cm² @Temperature -30.0 °C |
42.4 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) 25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p.. |